Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 800 °C | 1470 °F | |
Wieland 1005 Wilaform Gold Hard red gold alloy for used in decoration manufacturing.Applications: casting, chains, laminar decorationDental |
|||
Solidus | 800 °C | 1470 °F | |
Wieland 3012 Wilaform Silver A balance of manufacturing and performance characteristics makes this the preferential silver alloy in the decoration manufacturing industry. The alloy unites good ductility properties with the nec.. |