Thermal Properties Metric English Comments
Solidus 682 °C
1260 °F
Melting Point
Lucas-Milhaupt BRAZE 495 Carbide Brazing Alloy
Applications: Because of its excellent wetting properties, Braze 495 is used extensively for brazing tungsten carbide inserts to cutting tools and rock drills. It may be used for joining all types ..
Solidus 682 °C
1260 °F
Lucas-Milhaupt Silvaloy® A35 Brazing Alloy
Silvaloy A35 is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is used for brazing in the electrical industry and for brazing brass..