Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 640.6 °C | 1185 °F | Melting Point |
Lucas-Milhaupt SIL-FOS 2 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 2 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in servi.. |
|||
Solidus | 640.6 °C | 1185 °F | Melting Point |
Lucas-Milhaupt SIL-FOS 5 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 5 was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditionin.. |
|||
Solidus | 640.6 °C | 1185 °F | Melting Point |
Lucas-Milhaupt SIL-FOS 6 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 6 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in servi.. |
|||
Solidus | 640.6 °C | 1185 °F | Melting Point |
Lucas-Milhaupt SIL-FOS Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditioning .. |