Solidus 230 °C
446 °F
Johnson Matthey JM 97C Soft Solder/Flux
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi..
Solidus 230 °C
446 °F
Johnson Matthey JM 99C Soft Solder/Flux
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi..