Thermal Properties Metric English Comments
Solidus 211 °C
412 °F
Indium Corp. Indalloy® 249 91.8Sn/3.4Ag/4.8Bi Lead-Free Solder Alloy
Board & component metallizations must be Pb-free. U.S. Patent 5,439,639 (ICA Licensed Sandia Patent)Information provided by the manufacturer, Indium Corporation.