Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 181 °C | 358 °F | |
Indium Corp. Indalloy 226 Tin Solder Alloy Zinc causes high dross U.S. Patent #5,242,658; covers 72.8-89.4Sn 6.7-19.2Zn 2.7-16.4In; temp. range Liq.. 176-193, Sol. 166-191.4Information Provided by Indium Corporation |