Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 146 °C | 295 °F | |
Indium Corp. Indalloy 102 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 146 °C | 295 °F | |
AIM 97In/3Ag Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |