Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 1430 °C | 2610 °F | |
Astaras Anviloy® Weld Rod Anviloy® is a tungsten-based TIG filler metal used for enhancing and repairing dies and inserts. These weld rods work equally as well on both tool steel and tungsten based materials.Applications:R.. |
|||