Polymer Property : Solidus = 2530 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 1390 °C
2530 °F
Special Metals INCONEL® Alloy 751
A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-..
Solidus 1390 °C
2530 °F
Special Metals INCONEL® Alloy X-750
A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig..
Solidus 1390 °C
2530 °F
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700
This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels ..
Solidus 1390 °C
2530 °F
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600
This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels ..
Solidus 1390 °C
2530 °F
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603
This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels ..