Thermal Properties Metric English Comments
Solidus 245 °C
473 °F
Indium Corp. Indalloy® 233 Pb-Sb-Sn Solder Alloy
Intermediate temp solder. Creep resistant.Information provided by the manufacturer, Indium Corporation.