Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 1311 °C | 2392 °F | |
Special Metals INCOLOY® Alloy 925 A precipitation-hardenable nickel-iron-chromium alloy with additions of molybdenum and copper. It combines the high strength of a precipitation-hardenable alloy with the excellent corrosion resista.. |
|||
Solidus | 1311 °C | 2392 °F | |