Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 1232 °C | 2250 °F | |
Special Metals UDIMET® alloy R41 Ni-Cr Alloy UDIMET® alloy R41 (UNS N07041) is a precipitation-hardenable nickel-chromium alloy containing significant amounts of cobalt and molybdenum, along with lesser amounts of aluminum and titanium. Al.. |
|||
Solidus | 1230 °C | 2250 °F | |
Crucible Steel 321 Chromium-Nickel Steel Crucible 321 is a non-hardenable, low carbon austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures betwe.. |