Polymer Property : Solidus = 204 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 204 °C
399 °F
Indium Corp. Indalloy® 254 86.9Sn/10.0In/3.1Ag Lead-Free Solder Alloy
No Sn/In eutectic problem; potential use for flip chip assembly. Information provided by the manufacturer, Indium Corporation.