Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 993 °C | 1820 °F | |
Wall Colmonoy COLMONOY® 80 PTA - Nickel-Base Hard Surfacing Composite Powder Description: Colmonoy 80 PTA is a unique composite material containing a high volume percent of extremely abrasion resistant tungsten carbide particles (3500 DPH) in a soft (HRC 30) impact resistant.. |