Solidus 955 °C
1750 °F
Williams Advanced Alloys Wambraze™ WB955 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..
Solidus 955 °C
1750 °F
Williams Advanced Alloys Wambraze™ WB970 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..