Polymer Property : Solidus = 170 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 170 °C
338 °F
Indium Corp. Indalloy 111 Tin-Lead Solder Alloy
Information Provided by Indium Corporation