Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 880 °C | 1620 °F | |
Wieland 1605 Wilaform Gold Red gold for all kinds of decoration manufacturing.Applications: casting, laminar decoration, pipes, tubingDental |
|||
Solidus | 880 °C | 1620 °F | |
Williams Advanced Alloys Wambraze™ WB975 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |