Polymer Property : Solidus = 1340 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 727 °C
1340 °F
Melting Point
Lucas-Milhaupt BRAZE 541 Silver Based Cadmium Free Filler Metal
Characteristics:Braze 541 is an intermediate temperature silver brazing alloy with a rather long, 235EF (130EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting ..
Solidus 727 °C
1340 °F
Universal Wire Works BAg-13 (AMS 4772) Silver Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.