Solidus 1324 °C
2415 °F
Carlson GOC 276 Nickel-Molybdenum-Chromium
General DescriptionCarlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in ..