Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 1029 °C | 1885 °F | |
Cadi 2 MOLD-MOR™ A very hard heat treatable beryllium-copper alloy with moderate electrical conductivity. C17510 can be utilized when a combination of very good mechanical strength along with moderate electrical an.. |
|||
Solidus | 1029 °C | 1885 °F | |
Cadi 20 MOLD-MOR™ A Beryllium Copper Alloy with high thermal conductivity and moderate hardness.Information provided by Cadi Company. |
|||
Solidus | 1029 °C | 1885 °F | |
Cadi C17500 Copper Alloy Information provided by Cadi Company. |