Polymer Property : Solidus = 102 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 102 °C
216 °F
Indium Corp. Indalloy 52 Bismuth Solder Alloy
Information Provided by Indium Corporation
Solidus 102 °C
216 °F
Indium Corp. Indalloy 45 Bismuth Solder Alloy
Information Provided by Indium Corporation