Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 1000 °C | 1830 °F | |
Materion Beryllium Copper Alloy 10C Castings (UNS C82000) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchTabul.. |
|||
Solidus | 1000 °C | 1830 °F | |
Williams Advanced Alloys Wambraze™ WB1030 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |
|||
Solidus | 1000 °C | 1830 °F | |
Indium Corp. Indalloy 198 Silver-Gold Solder Alloy Information Provided by Indium Corporation |