Polymer Property : Thermal Conductivity = 97.9 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 14.1 W/m-K

@Temperature 200 °C
97.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Thermal Conductivity 14.1 W/m-K

@Temperature 300 °C
97.9 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 14.1 W/m-K

@Temperature 300 °C
97.9 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 14.1 W/m-K

@Temperature 300 °C
97.9 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 14.1 W/m-K

@Temperature 300 °C
97.9 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 14.1 W/m-K

@Temperature 300 °C
97.9 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 14.1 W/m-K

@Temperature 300 °C
97.9 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..