Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.44 - 1.64 W/m-K @Temperature 1600 °C |
9.99 - 11.4 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast CURAS 85 P Moldable Refractory Material Description: This phosphate bonded material based on corundum and bauxite has already at low temperature a reasonable strength and has a very good resistance against slag attack or liquid aluminum. .. |
|||
Thermal Conductivity | 1.44 - 1.64 W/m-K @Temperature 1600 °C |
9.99 - 11.4 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast CURAS 85 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This phosphate bonded material based on corundum and bauxite has a very go.. |
|||
Thermal Conductivity | 1.44 - 1.64 W/m-K @Temperature 1600 °C |
9.99 - 11.4 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast CURAS 85 PD GM Moldable Refractory Material Description: This material is supplied as a dry powder and can be gunned. This phosphate bonded material based on corundum and bauxite has a very good resistance against slag attack or liquid alumin.. |