Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.32 W/m-K @Temperature 100 °C |
9.16 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 53 E Dense Refractory Brick Description: Because of its very high erosion resistance this brick is applied in e.g. recirculation cyclones for CFB coal fired boilers.Remarks: This data represents average values, obtained from s.. |
|||
Thermal Conductivity | 1.32 W/m-K @Temperature 1100 °C |
9.16 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast B Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1300°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda.. |