Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 123.6 W/m-K @Temperature 200 °C |
857.8 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT)abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of p.. |