Polymer Property : Thermal Conductivity = 81.9 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Thermal Conductivity 11.8 W/m-K

@Temperature 25.0 °C
81.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..