Polymer Property : Thermal Conductivity = 81.2 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 11.7 W/m-K

@Temperature 100 °C
81.2 BTU-in/hr-ft²-°F

@Temperature 212 °F
Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy
INCONEL® alloy 740 is a nickel-chromium-cobalt alloy developed by Special Metals Corporation. The alloy is age hardenable by the precipitation of a gamma prime second phase. Potential applicati..