Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 80.0 W/m-K @Temperature 200 °C |
555 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that.. |