Thermal Properties Metric English Comments
Thermal Conductivity 1.07 - 1.27 W/m-K

@Temperature 1400 °C
7.43 - 8.81 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Gouda Vuurvast CURAS 60 SD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because this material contains a high percentage of sillimanite, it has a ..