Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 8.20 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 8.20 W/m-K

@Temperature 800 °C
56.9 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Zircar Ceramics Alumina Furnaceware
ZIRCAR Ceramics Alumina Furnaceware are high purity fully dense, fine grain aluminum oxide products suitable for use in applications with temperatures as high as 1800°C. Such uses include crucibles..
Copyright © lookpolymers.com All Rights Reserved