Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.17 W/m-K @Temperature 650 °C |
8.12 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast B Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1300°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda.. |