Thermal Conductivity 11.5 W/m-K

@Temperature 149 °C
79.8 BTU-in/hr-ft²-°F

@Temperature 300 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Thermal Conductivity 11.5 W/m-K

@Temperature 149 °C
79.8 BTU-in/hr-ft²-°F

@Temperature 300 °F
Haynes R-41 alloy, 0.635 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Thermal Conductivity 11.5 W/m-K

@Temperature 149 °C
79.8 BTU-in/hr-ft²-°F

@Temperature 300 °F
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Thermal Conductivity 11.5 W/m-K

@Temperature 149 °C
79.8 BTU-in/hr-ft²-°F

@Temperature 300 °F
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Thermal Conductivity 11.5 W/m-K

@Temperature 149 °C
79.8 BTU-in/hr-ft²-°F

@Temperature 300 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Thermal Conductivity 11.5 W/m-K

@Temperature 149 °C
79.8 BTU-in/hr-ft²-°F

@Temperature 300 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1121°C, air cooled, aged 16 hours at 899°C
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Thermal Conductivity 11.5 W/m-K

@Temperature 20.0 °C
79.8 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
ATI Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904)
Allegheny Ludlum AL 904 L™ Alloy (UNS N08904) is an austenitic stainless steel alloy designed for a middles to high level of corrosion resistance. The alloy is produced to low carbon levels for us..
Thermal Conductivity 11.5 W/m-K

@Temperature 149 °C
79.8 BTU-in/hr-ft²-°F

@Temperature 300 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include ..