Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 10.8 W/m-K @Temperature 100 °C |
75.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 10.8 W/m-K @Temperature 100 °C |
75.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 10.8 W/m-K @Temperature 100 °C |
75.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 10.8 W/m-K @Temperature 100 °C |
75.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 10.8 W/m-K @Temperature 100 °C |
75.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 10.8 W/m-K @Temperature 100 °C |
75.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |