Thermal Properties Metric English Comments
Thermal Conductivity 7.3995 W/m-K

@Temperature 23.0 °C
51.353 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Special Metals INCONEL® alloy 22 Austenitic Alloy
INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat..