Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.0585 W/m-K @Temperature 1000 °C |
7.3339 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 1.0585 W/m-K @Temperature 1000 °C |
7.3339 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |