Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 7.00 - 9.00 W/m-K @Temperature 1300 °C |
48.6 - 62.5 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo.. |