Polymer Property : Thermal Conductivity = 5.25 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.756 W/m-K

@Temperature 1600 °C
5.25 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Zircar Zirconia Buster Mat Alumina Insulation
Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga..
Thermal Conductivity 0.756 W/m-K

@Temperature 1600 °C
5.25 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Zircar Zirconia Buster Mat Alumina Insulation
Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga..