Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 45.0 W/m-K @Temperature 25.0 °C |
312 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (.. |