Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 6.00 W/m-K @Temperature 100 °C |
41.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 99 S Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qu.. |
|||
Thermal Conductivity | 6.00 - 8.00 W/m-K @Temperature 600 °C |
41.6 - 55.5 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo.. |
|||
Thermal Conductivity | 6.00 W/m-K @Temperature 1400 °C |
41.6 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 160 K Dense Vibrating Refractory Castable Description: Vibron 160 K is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity and high abrasion resistance. The thermal shock resistance is excell.. |
|||
Thermal Conductivity | 6.00 W/m-K @Temperature 100 °C |
41.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast LP 100 Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qual.. |