Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.560 - 0.660 W/m-K @Temperature 1000 °C |
3.89 - 4.58 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast CURON 120 C Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat.. |
|||
Thermal Conductivity | 0.560 - 0.660 W/m-K @Temperature 600 °C |
3.89 - 4.58 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 130 Dense Refractory Castable Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap.. |
|||
Thermal Conductivity | 0.560 - 0.660 W/m-K @Temperature 600 °C |
3.89 - 4.58 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 140 Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo.. |
|||
Thermal Conductivity | 0.560 - 0.660 W/m-K @Temperature 100 °C |
3.89 - 4.58 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 150 AC Dense Refractory Castable Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |