Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 48.6 W/m-K @Temperature 20.0 °C |
337 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Latrobe CBS-600™ VIM-VAR Carburizing Bearing and Gear Steel CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe.. |