Thermal Conductivity 33.4 W/m-K

@Temperature 10.0 °C
232 BTU-in/hr-ft²-°F

@Temperature 50.0 °F
Schmolz + Bickenbach Cryodur® 2510 (O-1) Cold Work Die Steel
Description: Cyrodur ® 2510 is a single melt Extra Fine Structure (EFS) material; and Supplied in the soft annealed conditionCharacteristics: Excellent dimensional stability during heat treatment; ..