Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 32.1 W/m-K @Temperature 500 °C |
223 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |
|||
Thermal Conductivity | 32.1 W/m-K @Temperature 100 °C |
223 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |