Thermal Properties Metric English Comments
Thermal Conductivity 32.0 W/m-K

@Temperature 599 °C
222 BTU-in/hr-ft²-°F

@Temperature 1110 °F
hardness of 45 HRC
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel
Description: Uddeholm Dievar is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross cracking, hot wear and plastic..
Thermal Conductivity 32.0 W/m-K

@Temperature 20.0 °C
222 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Assab Steels DF-3 Cold Work Steel
DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil..
Thermal Conductivity 32.0 W/m-K

@Temperature 600 °C
222 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..
Thermal Conductivity 32.0 W/m-K

@Temperature 400 °C
222 BTU-in/hr-ft²-°F

@Temperature 752 °F
Assab Steels QRO 90 SUPREME Hot Work Steel
QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista..
Thermal Conductivity 32.0 W/m-K

@Temperature 343 °C
222 BTU-in/hr-ft²-°F

@Temperature 650 °F
Schmolz + Bickenbach Cryodur® 2510 (O-1) Cold Work Die Steel
Description: Cyrodur ® 2510 is a single melt Extra Fine Structure (EFS) material; and Supplied in the soft annealed conditionCharacteristics: Excellent dimensional stability during heat treatment; ..
Thermal Conductivity 32.0 W/m-K

@Temperature 20.0 °C
222 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
hardened to 62 HRC
Bohler-Uddeholm O1 Cold Work Tool Steel
Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha..