Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 30.4 W/m-K @Temperature 500 °C |
211 BTU-in/hr-ft²-°F @Temperature 932 °F |
Hardened and tempered |
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Thermal Conductivity | 30.4 W/m-K @Temperature 200 °C |
211 BTU-in/hr-ft²-°F @Temperature 392 °F |
Hardened and tempered |
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |