Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 30.238 W/m-K @Temperature 1150 °C |
209.85 BTU-in/hr-ft²-°F @Temperature 2100 °F |
|
Special Metals INCOLOY® alloy 832 Stainless Steel INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula.. |