Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.80 W/m-K @Temperature 1100 °C |
26.4 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 99 S Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qu.. |
|||
Thermal Conductivity | 3.80 W/m-K @Temperature 1100 °C |
26.4 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast LP 100 Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qual.. |
|||
Thermal Conductivity | 3.80 W/m-K @Temperature 650 °C |
26.4 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast LP 97-3 Dense Refractory Brick Description: A high alumina quality brick containing a limited percentage of chromium oxide for improved slag resistance. The product has a very low silica- and iron oxide percentage so that it can .. |