Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.5234 W/m-K @Temperature 260 °C |
3.627 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |