Polymer Property : Thermal Conductivity = 3.40 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 3.40 W/m-K

@Temperature 1100 °C
23.6 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AC 85-10 D Dense Refractory Brick
Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te..
Thermal Conductivity 3.40 W/m-K

@Temperature 650 °C
23.6 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 99 Dense Refractory Brick
Description: This high purity alumina based brick finds wide application in chemical reactors. The low percentages of SiO2 and Fe2O3 makes this brick very resistant in reducing conditions.Remarks: T..
Thermal Conductivity 3.40 W/m-K

@Temperature 1100 °C
23.6 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 99 Dense Refractory Brick
Description: This high purity alumina based brick finds wide application in chemical reactors. The low percentages of SiO2 and Fe2O3 makes this brick very resistant in reducing conditions.Remarks: T..